Kekere asiwaju C17300

Asiwaju kekere yii C17300 pẹlu Pb<0.1%, ṣugbọn iṣẹ gige rẹ jẹ kanna bi C17300.


Alaye ọja

ọja Tags

Ọja naa ti ni ipin bi awọn ọja imọ-ẹrọ giga (ẹka ohun elo tuntun) ni Agbegbe Jiangsu lati ọdun 2013. O gba imọ-ẹrọ ilana kukuru (awọn itọsi 6) pẹlu awọn ẹtọ ohun-ini ominira ti ominira, eyiti o ni ibẹrẹ ni idagbasoke agbara-giga giga-giga-ọfẹ ọfẹ- gige ga konge beryllium Ejò opa ati titi abele gbára ipo iṣe ti akowọle awọn superior ga-kikankikan ga-conductivity free-Ige ga konge beryllium Ejò opa.Lọwọlọwọ, awọn alabara mẹfa wa ni ipo ni Top 10 Awọn iṣelọpọ ti Asopọ-igbohunsafẹfẹ Redio Agbaye.

Yi kekere asiwajuC17300pẹlu Pb | 0.1%, ṣugbọn iṣẹ gige rẹ jẹ kanna bi C17300.

1. Kemikali Tiwqn ti kekere asiwaju C17300

Awoṣe

Be

Ni+Co

Ni+Co+Fe

Pb

Cu

C17300

1.8-2.0

≥0.20

≤0.6

0.1

Iyokù

2. Ti ara Ati Mechanical Properties ofkekere asiwajuC17300

Ìpínlẹ̀
(gẹgẹ bi ASTM)

Ooru Itọju
(℃)

Iwọn opin

(mm)

Agbara Fifẹ (MPa)

Agbara Ikore (MPa)

Ilọsiwaju

4xD(%)

Lile

Electrical Conductivity

(IACS,%)

HV0.5

HRB tabi HRC

TB00

775℃ ~ 800℃

Gbogbo

410-590

140

20

159-162

B45-B85

15-19

TD04

775℃~800℃ Solusan+Ilana ilana tutu

8-20

620-860

520

8

175-257

B88-B102

15-19

0.6-8

620-900

520

8

175-260

B88-B103

TH04

315 ℃x1 ~ 2 wakati

8-20

1140-1380

930

20

345-406

C27-C44

23-28

0.6-8

1210-1450

1000

:4

354-415

C38-C45

3. Ige Performance ofkekere asiwajuC17300
Ni deede si 65% ti ẹrọ ti idẹ C3600

4. Ohun elo Fields ofkekere asiwajuC17300
O jẹ lilo ni akọkọ ni asopo coaxial, iwadii, ibaraẹnisọrọ, afẹfẹ ologun