Al2O3 pipinfa Agbara Blowed Blowed dì (C15715, C15725, C15760)
* Pitita pipin funni ni agbara ti o dara julọ ni idari ti o dara julọ ni afikun imurasile ti o ga julọ.
* Agbara giga wa ati ṣiṣe kaakiri Al2O3 ti o funni ni awọn ọpá Awọn Aṣọ Awọn ọpá ṣe nitori awọn olupese iṣẹ ti o ga julọ .A yiyi ọja ti o pari
* O nṣe ayẹwo bi ọja-ipa-imọ-ẹrọ Jiiangsu (fun kilasi awọn ohun elo tuntun) ni ọdun 2013
* Awọn papawi meji ti ni a ti fun ni.The ile-iṣẹ jẹ iduro t'olofin fun fifa kaakiri Al2O3 pinpin awọn ọpá V2O, boṣewa ti orilẹ-ede fun ile-iṣẹ naa.
1
Awoṣe | Cu + AG | Al2O3 | Ala | Ob | P | Fe | Pb |
C15715 | ≥99.45 | 0.25-0.32 | ≤0.03 | ≤0.015 | ≤0.003 | ≤0.01 | ≤0.01 |
C15725 | ≥99.25 | 0.43-0.51 | ≤0.03 | ≤0.015 | ≤0.003 | ≤0.01 | ≤0.01 |
C15760 | ≥98.55 | 0.10-0.20 | ≤0.03 | ≤0.015 | ≤0.003 | ≤0.01 | ≤0.01 |
aAl ti o wa ni fọọmu miiran ju al2O3 | |||||||
bO ti o wa ni fọọmu miiran ju al2O3 |
2.
Iwọn opin | Gbipa gbigbin | Ipọn | Iwọn opin | ||||
50-100 | 0.103 | ≤100 | > 100-200 | > 200-300 | > 300-400 | > 400-600 | |
> 100-200 | ± 004 | Iyapa ti o ni iyanilenu ti sisanra | |||||
> 200-300 | ± 005 | 10-20 | ± 0.30 | ± 035 | ± 040 | ± 045 | 0.50 |
> 300-400 | ± 006 | > 20-30 | ± 035 | ± 040 | ± 045 | 0.50 | ± 055 |
3. Awọn ohun-ini ti ara ati ẹrọ ti pipinka Al2O3 lagbara
Awoṣe | Ipo | Tensele Agbara RM (MPA) | Afikun ipa-agbara ṣiṣu Rp0.2 (MPPA) |
| Rockwell lile HRB | Iwọn didun metacne (Ω * MM2 / M) | Itanna itanna (Iacs,%) | Itanna itanna (Ms / m) |
C15715 | H04 | ≥427 | ≥407 | ≥14 | ≥63 | ≤0.0184 | ≥92 | ≥53.4 |
C15725 | H04 | ≥483 | ≥448 | ≥12 | ≥77 | ≤0.01937 | ≥89 | ≥51.6 |
C15760 | H04 | ≥552 | ≥517 | ≥10 | ≥83 | ≤0.02210 | ≥78 | ≥45.2 |
4. Awọn aaye ohun elo ti pipinka Al2O3 lagbara
O ti lo ni kikun fun awọn ile-iṣẹ ile-iṣẹ